PROBLEM:
Small trappings of air are visible (pinholes).
Cause Solution
Ink Ink is too thick. Add thinner to ink.
Ink has jelly-like consistency; doesn't flow. Add flow agent FX 32
(TTA #1205001)
Pad Pad has a cut or holes in pad. Reposition or replace pad.
Pad is too flat. Use a pad with a sharper angle.
Pad is contaminated. Clean pad with pad cleaner (TTA #1411121) or clear tape.
Cliché (plate) Etch is too deep. Remake cliché to the proper etch depth.
Cliché has wrong style of etch for the application. When using a flat or soft pad, the cliché should be screened.
Material (substrate) Parts are contaminated with dust. Clean parts.
Parts have texture. Use a hard pad with a sharp angle. It may be necessary to dry ink on pad to bridge the texture.
Other Film is not clean.



Pinholes show in film positive.
Clean the film before making temporary clichés witn anti-static film cleaner (TTA#1411134)
Retouch image on positive; then make a new cliché.
Back to Troubleshooting Guide Q & A

Download a PDF of entire
Troubleshooting Guide


Download a PDF of entire
Troubleshooting Guide en Espanol



Home
| Consumables | Machines | Support | What's New | Specialty | Trade Shows | Contact Us

© 2006 ITW Trans TechAn Illinois Tool Works Company